Nano Bond Additive 123

Product Description: Nano Bond Additive is a fusion additive that is designed to use with many various types of metallic clay materials such as, magnesium, calcium, gypsum, aluminum, and most non-metallic clays. Nano Bond Additive is designed to increase bonding and flexural strength.  Each clay material will produce a different type of bonding and curing strength depending on the type and various blends of clay materials.  This is also dependent on the amount of Nano Bond Additive material used.

Technology: Nano Bond Additive is a Hi-Tech water based additive fusion with Nano molecular polymer technology to impregnate into micro particles of clay, gypsum, calcium, silica, mica, perlites, ceramics, all natural minerals, quartz, and most synthetic micro mineral clay-based materials.  This technology permanently alters the original state of micro particles integrally by reactive fusion technology and enhances their outlook and performance.

Performance Characters: Nano Bond Additive is simplified to use with most clay and synthetic dry blends. Use 2 to 4 floz per one pound of dry mix. Nano Bond Additive is a non-reactive and safe to use in conjunction with most bonding agents and additives. Improves moisture requirements while curing. Nano Bond Additive has time-release mechanism that allows precise amount of moisture requirement for initial and final cure. Cured and finish product surface can be painted or sealed with most commonly available products. Also it is safe to use with most mineral base pigments and is designed to use with clay base products.

Intended Use:

  • Light weight clay products
  • Pre cast panels
  • Lightweight dry wall products
  • Stucco and pre- fabricated stucco panels
  • Light weight clay statuaries
  • Many specialty clay products
  • Mortar add mixes for grouts and mortar joints

Benefits And Compliances:

  • Improves green strength
  • Increase PSI
  • Increase flexural strength, Compliances with “standard test method for evaluating masonry bond strength”. ASTM C 1357.
  • Increase compressive strength, Compliances with “standard test method for constructing and testing masonry prisms used to determine compliance with specified compressive strength of masonry. ASTM C1314.
  • Compliances with “standard test method for drying shrinkage (CMU). ASTM C 426.
  • Reduces air pockets faster for pre cast systems for smoother finish.
  • Water per-menace of masonry, Compliances with ASTM E and ASTM E 514-74 capable of achieving of a class E rating when test extends to 72 hours.
  • Improves water per-menace of masonry, compliances with “standard test method for water penetration and leakage threw masonry.” ASTM E 514.
  • Also compliances with ASTM C-1059 type 2, ASTM C 1042 type 2, ASTM 404 size No2, ASTM-C 144, and V.O.C. compliant.
  • It meets and exceeds compliance test method, ASTM burn test requirements at 2000°F for 1, 2, 3, and 4 hour test.
  • Compliances with UL Test requirements.

Limitation: Keep from freezing. Store product at room temperature. Do not mix this product with other chemicals only use as directed.

Storage And Handling: Store this product between 45°F to 80°F for maximum self-life of one year. Keep container close after each use. Light agitation may require after long period of storage. Mix well before use.

Spills And Cleaning: For small spills use warm water and mop to clean floor. For large spills, contained effected areas use wet vacuums to pump excess spills. Rinse or mop floors with clean water. Keep spill from entering floor drains. Product may clog drainpipes. Clean all handling equipments with soap and warm water.

Warning: Keep out of reach of children.

Precautions: For personal safety, use rubber gloves and eye protections. Use clean hygiene practice. For prolong skin contact, rinse effected areas with warm water and soap. For accidental eye contact, flush eyes with cold water for 10 minutes. If accidentally indigested, do not induce vomiting drink cold water and consult physician for proper care and treatment.